Corrosion resistance
It exhibits strong corrosion resistance to the atmosphere, fresh water, acidic solutions (such as acetic acid, nitric acid) and weak alkaline environments at room temperature, and is particularly suitable for food processing equipment, chemical pipelines and other scenarios. Avoid contact with chloride ion media (such as seawater) to prevent local corrosion.
Mechanical properties
Tensile strength ≥ 620MPa, yield strength ≥ 310MPa, elongation up to 46.7%, with both high temperature strength and creep resistance, can be used for a short period of time at 1000-1200℃.
Processing performance
It can be processed into round bars, hexagonal bars and other forms through hot rolling, cold drawing, grinding and other processes, with high surface gloss and no magnetism. Solution treatment (1010-1150℃ fast cooling) is required after welding to optimize corrosion resistance. Common processing methods include TIG welding, MIG welding, etc.
Application scenarios
It is widely used in food equipment, medical equipment, chemical pipelines, architectural decoration and other fields, with a typical specification range of Φ1.0-20.0mm
Product Name | Stainless Steel Bar |
Standard | ASTM,JIS,DIN,GB,AISI,DIN,EN |
Material | 201, 202, 301, 301L, 304, 304L, 316, 316L, 321, 310S, 904L, 410, 420J2, 430, 2205, 2507, 321H, 347, 347H, 403, 405, 409, 420, 430, 631, 904L, 305, 301L, 317, 317L, 309, 309S 310 |
Technique | Cold drawn, Hot rolled, Cold rolled and Others. |
Diameter | 6-12mm or Customizable |
Length | 1000 – 6000mm or Customizable |
Surface Treatment | BA/2B/NO.1/NO.3/NO.4/8K/HL/2D/1D |
Origin | China |
HS Code | 7220204000 |
Delivery Time | {Delivery Time} |
After-sales Service | 24 hours online |
Production Capacity | {Production Capacity} |
Price Terms | EXW, FOB, CIF, CRF, CNF or others |
Loading Port | {Port} |
Payment Term | TT, LC, Cash, Paypal, DP, DA, Western Union or Others. |
Application | 1. Tableware, cabinets, indoor pipelines, water heaters, boilers, bathtubs |
2. Automotive parts | |
3.Medicale quipment, building materials, chemicals, food industry, agriculture, ship components, etc. | |
Packaging | Bundle, PVC Bag, Nylon Belt, Cable Tie, Standard export seaworthy package or as Request. |
Processing Service | Bending, Welding, Decoiling, Punching, Cutting and Others. |
Tolerance | ±1% |
MOQ | {MOQ} |
Composition of Stainless Steel
Steel is an alloy of iron and carbon. Stainless steels are steels containing at least 10.5% chromium, less than 1.2% carbon and other alloying elements. Stainless steel’s corrosion resistance and
mechanical properties can be further enhanced by adding other elements, such as nickel, molybdenum, titanium, niobium, manganese, etc.
Grade | C | Si | Mn | P | S | Cr | Ni | Mo | N | Cu |
201 | ≤0.15 | ≤0.75 | 5.5~7.5 | ≤0.060 | ≤0.03 | 16.00~18.00 | 3.5~5.5 | – | – | 0.08 |
202 | ≤0.15 | ≤1.00 | 7.5~10.00 | ≤0.060 | ≤0.03 | 17.00~19.00 | 4.0~6.0 | – | ≤0.25 | |
301 | ≤0.15 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 16.00~18.00 | 6.00~8.00 | – | ||
302 | ≤0.15 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.03 | 17.00~19.00 | 8.00~10.00 | – | ||
304 | ≤0.07 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 18.00~20.00 | 8.00~10.50 | – | ||
304L | ≤0.030 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 18.00~20.00 | 9.00~13.00 | – | ||
310S | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 24.00~26.00 | 19.00~22.00 | – | ||
316 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 16.00~18.00 | 10.00~14.00 | 2.00~3.00 | ||
316L | ≤0.03 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 16.00~18.00 | 12.00~15.00 | 2.00~3.00 | ||
321 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 17.00~19.00 | 9.00~13.00 | – | ||
430 | ≤0.12 | ≤0.75 | ≤1.00 | ≤0.040 | ≤0.03 | 16.00~18.00 | – | |||
2205 | ≤0.03 | ≤1.00 | ≤2.00 | ≤0.030 | ≤0.015 | 22.00~23.00 | 4.5~6.5 | 2.5~3.5 | ||
2507 | ≤0.03 | ≤0.08 | ≤1.20 | ≤0.035 | ≤0.015 | 24.00~26.00 | 6.00~8.00 | 3.0~5.0 | ||
904L | ≤0.02 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.035 | 19.00~23.00 | 23.00~28.00 | 4.0~5.0 | 1.0~2.0 | |
INCONEL028 | ≤0.03 | ≤1.00 | ≤2.50 | ≤0.030 | ≤0.030 | ≤28.0 | ≤34.0 | ≤4.0 | ≤1.4 | |
MONEL400 | ≤0.30 | ≤0.5 | ≤2.00 | – | ≤0.024 | – | ≥63.0 | – | ≤34.0 | |
INCONEL800 | ≤0.10 | ≤1.00 | ≤1.50 | – | ≤0.015 | ≤23.0 | ≤35 | 4.0~5.0 | – | ≤0.75 |