SS 321 Stainless steel bar bars

SS321 stainless steel is a stabilized austenitic stainless steel with a titanium addition of at least 5 times the carbon content. The addition of titanium reduces or prevents the sensitization of carbide precipitation during welding and when used in the 425-815°C temperature range. It also improves certain properties at elevated temperatures. SS321 has excellent resistance to oxidation and corrosion and has good creep strength. It is primarily used in oil refining equipment, pressure vessel piping, radiant superheaters, bellows, and high temperature heat treatment equipment

The characteristics of SS321 stainless steel bar are as follows:

High temperature resistance: It has excellent high temperature resistance and can withstand corrosion and oxidation in high temperature environment for a long time.

Corrosion resistance: It has excellent corrosion resistance and can resist corrosion in many chemical environments, including organic acids, alkalis and solvents.

Oxidation resistance: It has good oxidation resistance and can resist high temperature oxidation and extend service life.

Processing performance: It has good plasticity and weldability and is easy to process into various shapes and sizes.

Mechanical properties: It has high tensile strength, yield strength and impact toughness, suitable for various engineering and structural applications.

Chemical element composition content: The chemical element composition content of SS321 stainless steel includes chromium (Cr), nickel (Ni), iron (Fe) and titanium (Ti). The proportion and combination of these elements give SS321 stainless steel high temperature resistance, corrosion resistance and oxidation resistance 3.

Strength and hardness: It has relatively high strength and hardness, which makes it perform well in some applications that require high strength and compressive resistance 1.

Ductility and stress fracture resistance: Compared with 304 alloy, it has better ductility and stress fracture resistance, and has better creep stress resistance and stress fracture resistance1.

Organization structure: As a duplex stainless steel, the organization structure of SS321 contains austenite phase and ferrite phase, which makes it have good corrosion resistance and strength1.

Application field: It is commonly used in chemical equipment, petrochemical equipment, food industry equipment and other fields under high temperature. It can also be used in aircraft, exhaust pipes, boiler drums, etc.; it is also widely used in chemical, petroleum and pharmaceutical fields.

 

Product   Name Barre en acier inoxydable
Standard ASTM,JIS,DIN,GB,AISI,DIN,EN
Matériau 201, 202, 301, 301L, 304, 304L, 316, 316L, 321, 310S, 904L, 410, 420J2, 430, 2205, 2507, 321H, 347, 347H, 403, 405, 409, 420, 430, 631, 904L, 305, 301L, 317, 317L, 309, 309S 310
Technique Etiré à froid, laminé à chaud, laminé à froid et autres.
Diameter 6-12mm ou personnalisable
Longueur 1000 – 6000mm or Customizable
Traitement de surface BA/2B/NO.1/NO.3/NO.4/8K/HL/2D/1D
Origine Chine
Code SH 7220204000
Délai de livraison {Délai de livraison}
Service après-vente 24 heures en ligne
Capacité de production {Capacité de production}
Conditions de prix EXW, FOB, CIF, CRF, CNF or   others
Port de chargement {Port}
Délai de paiement TT, LC, Cash, Paypal, DP, DA,   Western Union or Others.
Application 1. Vaisselle, armoires, canalisations intérieures, chauffe-eau, chaudières, baignoires
2. Pièces automobiles
3. équipements médicaux, matériaux de construction, produits chimiques, industrie alimentaire, agriculture, composants de navires, etc.
Emballage Emballage, sac en PVC, ceinture en nylon, serre-câble, emballage maritime standard pour l'exportation ou selon la demande.
Service de traitement Pliage, soudage, décochage, poinçonnage, découpage et autres.
Tolérance ±1%
MOQ {MOQ}

Composition de l'acier inoxydable

L'acier est un alliage de fer et de carbone. Les aciers inoxydables sont des aciers contenant au moins 10,5% de chrome, moins de 1,2% de carbone et d'autres éléments d'alliage. La résistance à la corrosion de l'acier inoxydable et

Les propriétés mécaniques peuvent être encore améliorées par l'ajout d'autres éléments, tels que le nickel, le molybdène, le titane, le niobium, le manganèse, etc.

Grade C Si Mn P S Cr Ni Mo N Cu
201 ≤0.15 ≤0.75 5.5~7.5 ≤0.060 ≤0.03 16.00~18.00 3.5~5.5 0.08
202 ≤0.15 ≤1.00 7.5~10.00 ≤0.060 ≤0.03 17.00~19.00 4.0~6.0 ≤0.25
301 ≤0.15 ≤1.00 ≤2.00 ≤0.045 ≤0.03 16.00~18.00 6.00~8.00
302 ≤0.15 ≤1.00 ≤2.00 ≤0.035 ≤0.03 17.00~19.00 8.00~10.00
304 ≤0.07 ≤1.00 ≤2.00 ≤0.045 ≤0.03 18.00~20.00 8.00~10.50
304L ≤0.030 ≤1.00 ≤2.00 ≤0.045 ≤0.03 18.00~20.00 9.00~13.00
310S ≤0.08 ≤1.00 ≤2.00 ≤0.045 ≤0.03 24.00~26.00 19.00~22.00
316 ≤0.08 ≤1.00 ≤2.00 ≤0.045 ≤0.03 16.00~18.00 10.00~14.00 2.00~3.00
316L ≤0.03 ≤1.00 ≤2.00 ≤0.045 ≤0.03 16.00~18.00 12.00~15.00 2.00~3.00
321 ≤0.08 ≤1.00 ≤2.00 ≤0.045 ≤0.03 17.00~19.00 9.00~13.00
430 ≤0.12 ≤0.75 ≤1.00 ≤0.040 ≤0.03 16.00~18.00
2205 ≤0.03 ≤1.00 ≤2.00 ≤0.030 ≤0.015 22.00~23.00 4.5~6.5 2.5~3.5
2507 ≤0.03 ≤0.08 ≤1.20 ≤0.035 ≤0.015 24.00~26.00 6.00~8.00 3.0~5.0
904L ≤0.02 ≤1.00 ≤2.00 ≤0.045 ≤0.035 19.00~23.00 23.00~28.00 4.0~5.0 1.0~2.0
INCONEL028 ≤0.03 ≤1.00 ≤2.50 ≤0.030 ≤0.030 ≤28.0 ≤34.0 ≤4.0 ≤1.4
MONEL400 ≤0.30 ≤0.5 ≤2.00 ≤0.024 ≥63.0 ≤34.0
INCONEL800 ≤0.10 ≤1.00 ≤1.50 ≤0.015 ≤23.0 ≤35 4.0~5.0 ≤0.75

 

 