SS 409 Stainless steel plate sheet

The main advantages of SS 409 stainless steel are its high temperature strength and oxidation resistance, and it can withstand repeated heating below 980°C. It can maintain good strength and toughness at high temperatures, and has excellent heat resistance and corrosion resistance. In addition, 409 SS stainless steel also has good processing performance and weldability, and is widely used in chemical, petroleum, aviation, nuclear energy and other fields. Due to its lower carbon content, 409 SS stainless steel can reduce the precipitation of carbides during welding, thereby reducing the risk of intergranular corrosion, and is suitable for occasions that require welding.

SS409 stainless steel (ferritic stainless steel) has the following characteristics:

Corrosion resistance
It has good resistance to most corrosive media such as acids, alkalis, and salts at room temperature, and remains stable in high temperature environments. However, it should be used with caution in chlorine-containing environments. ‌

High temperature performance
It can withstand repeated heating below 980°C, and still maintain strength and toughness at high temperatures (about 1370-1400°C), which is suitable for high-temperature scenes such as exhaust systems and burners. ‌

Processing performance
It is easy to cut, weld and form. During processing, attention should be paid to cleanliness to avoid contamination. The risk of carbide precipitation during welding is low, which is suitable for complex structure manufacturing. ‌

Mechanical properties
Tensile strength is about 490 MPa, yield strength ≥900 MPa, elongation ≥15%, and it has both strength and plasticity. ‌

Cost and applicability
The cost is lower than that of 300 series stainless steel. It is widely used in scenes such as automotive exhaust systems, building decoration, and chemical equipment, but the surface is easily scratched. ‌

 

Product   Name Stainless Steel Plate/Sheet
Standard ASTM,JIS,DIN,GB,AISI,DIN,EN
Matériau 201, 202, 301, 301L, 304, 304L, 316, 316L, 321, 310S, 904L, 410, 420J2, 430, 2205, 2507, 321H, 347, 347H, 403, 405, 409, 420, 430, 631, 904L, 305, 301L, 317, 317L, 309, 309S 310
Technique Etiré à froid, laminé à chaud, laminé à froid et autres.
Largeur 6-12mm ou personnalisable
Épaisseur 1-120mm or Customizable
Longueur 1000 – 6000mm or Customizable
Traitement de surface BA/2B/NO.1/NO.3/NO.4/8K/HL/2D/1D
Origine Chine
Code SH 7211190000
Délai de livraison {Délai de livraison}
Service après-vente 24 heures en ligne
Capacité de production {Capacité de production}
Conditions de prix EXW, FOB, CIF, CRF, CNF or   Others
Port de chargement {Port}
Délai de paiement TT, LC, Cash, Paypal, DP, DA, Western Union ou autres.
Application 1. Architectural decoration.   Such as exterior walls, curtain walls, ceilings, stair handrails, doors and   windows, etc.
2.   Kitchen furniture. Such as kitchen stove, sink, etc.
3.   Chemical equipment. Such as containers, pipelines, etc.
4. Food   processing. Such as food containers, processing tables, etc.
5.   Automobile manufacturing. Such as vehicle body, exhaust pipe, fuel tank, etc.
6.   Electronic devices. Such as manufacturing casings, structural components,   etc. for electronic devices.
7.   Medical equipment. Such as surgical instruments, surgical instruments,   medical utensils, etc.
8.   Shipbuilding. Such as ship hulls, pipelines, equipment supports, etc.
Emballage Emballage, sac en PVC, ceinture en nylon, serre-câble, emballage maritime standard pour l'exportation ou selon la demande.
Service de traitement Pliage, soudage, décochage, poinçonnage, découpage et autres.
Tolérance ±1%
MOQ {MOQ}

 

Composition de l'acier inoxydable

L'acier est un alliage de fer et de carbone. Les aciers inoxydables sont des aciers contenant au moins 10,5% de chrome, moins de 1,2% de carbone et d'autres éléments d'alliage. La résistance à la corrosion de l'acier inoxydable et

Les propriétés mécaniques peuvent être encore améliorées par l'ajout d'autres éléments, tels que le nickel, le molybdène, le titane, le niobium, le manganèse, etc.

Grade C Si Mn P S Cr Ni Mo N Cu
201 ≤0.15 ≤0.75 5.5~7.5 ≤0.060 ≤0.03 16.00~18.00 3.5~5.5 0.08
202 ≤0.15 ≤1.00 7.5~10.00 ≤0.060 ≤0.03 17.00~19.00 4.0~6.0 ≤0.25
301 ≤0.15 ≤1.00 ≤2.00 ≤0.045 ≤0.03 16.00~18.00 6.00~8.00
302 ≤0.15 ≤1.00 ≤2.00 ≤0.035 ≤0.03 17.00~19.00 8.00~10.00
304 ≤0.07 ≤1.00 ≤2.00 ≤0.045 ≤0.03 18.00~20.00 8.00~10.50
304L ≤0.030 ≤1.00 ≤2.00 ≤0.045 ≤0.03 18.00~20.00 9.00~13.00
310S ≤0.08 ≤1.00 ≤2.00 ≤0.045 ≤0.03 24.00~26.00 19.00~22.00
316 ≤0.08 ≤1.00 ≤2.00 ≤0.045 ≤0.03 16.00~18.00 10.00~14.00 2.00~3.00
316L ≤0.03 ≤1.00 ≤2.00 ≤0.045 ≤0.03 16.00~18.00 12.00~15.00 2.00~3.00
321 ≤0.08 ≤1.00 ≤2.00 ≤0.045 ≤0.03 17.00~19.00 9.00~13.00
430 ≤0.12 ≤0.75 ≤1.00 ≤0.040 ≤0.03 16.00~18.00
2205 ≤0.03 ≤1.00 ≤2.00 ≤0.030 ≤0.015 22.00~23.00 4.5~6.5 2.5~3.5
2507 ≤0.03 ≤0.08 ≤1.20 ≤0.035 ≤0.015 24.00~26.00 6.00~8.00 3.0~5.0
904L ≤0.02 ≤1.00 ≤2.00 ≤0.045 ≤0.035 19.00~23.00 23.00~28.00 4.0~5.0 1.0~2.0
INCONEL028 ≤0.03 ≤1.00 ≤2.50 ≤0.030 ≤0.030 ≤28.0 ≤34.0 ≤4.0 ≤1.4
MONEL400 ≤0.30 ≤0.5 ≤2.00 ≤0.024 ≥63.0 ≤34.0
INCONEL800 ≤0.10 ≤1.00 ≤1.50 ≤0.015 ≤23.0 ≤35 4.0~5.0 ≤0.75