Corrosion resistance
Contains high chromium (22%-24%) and nickel (12%-15%) elements, forming a dense oxide film, which can protect the steel surface in high temperature and corrosive environments, and has better corrosion resistance than SUS304 stainless steel.
Heat resistance
Can withstand repeated heating below 980℃, and still maintain strength and toughness at high temperatures, suitable for 800-1000℃ working environments.
Processing performance
Adding sulfur elements, the friction during cutting is small, the surface finish is high, and it is suitable for precision processing.
Applicable scenarios
Widely used in high temperature and high pressure scenarios such as boilers, industrial furnaces, and chemical equipment, and also suitable for precision machining.
Product Name | Stainless Steel Ber |
Estándar | ASTM,JIS,DIN,GB,AISI,DIN,EN |
Material | 201, 202, 301, 301L, 304, 304L, 316, 316L, 321, 310S, 904L, 410, 420J2, 430, 2205, 2507, 321H, 347, 347H, 403, 405, 409, 420, 430, 631, 904L, 305, 301L, 317, 317L, 309, 309S 310 |
Técnica | Estirado en frío, Laminado en caliente, Laminado en frío y Otros. |
Diameter | 6-12 mm o personalizable |
Longitud | 1000 – 6000mm or Customizable |
Tratamiento de superficies | BA/2B/NO.1/NO.3/NO.4/8K/HL/2D/1D |
Origen | China |
Código SA | 7220204000 |
Plazo de entrega | {Tiempo de entrega} |
Servicio posventa | 24 horas en línea |
Capacidad de producción | {Capacidad de producción} |
Condiciones de precio | EXW, FOB, CIF, CRF, CNF or others |
Puerto de carga | {Puerto} |
Plazo de pago | TT, LC, Cash, Paypal, DP, DA, Western Union or Others. |
Aplicación | 1. Vajilla, armarios, tuberías interiores, calentadores de agua, calderas, bañeras |
2. Piezas de automóvil | |
3. Equipamiento médico, materiales de construcción, productos químicos, industria alimentaria, agricultura, componentes navales, etc. | |
Embalaje | Paquete, bolsa de PVC, cinturón de nylon, atadura de cables, paquete marítimo de exportación estándar o como petición. |
Servicio de tramitación | Doblado, soldadura, desbobinado, punzonado, corte y otros. |
Tolerancia | ±1% |
MOQ | {MOQ} |
Composición del acero inoxidable
El acero es una aleación de hierro y carbono. Los aceros inoxidables son aceros que contienen al menos 10,5% de cromo, menos de 1,2% de carbono y otros elementos de aleación. La resistencia a la corrosión del acero inoxidable y
Las propiedades mecánicas pueden mejorarse aún más añadiendo otros elementos, como níquel, molibdeno, titanio, niobio, manganeso, etc.
Grado | C | Si | Mn | P | S | Cr | Ni | Mo | N | Cu |
201 | ≤0.15 | ≤0.75 | 5.5~7.5 | ≤0.060 | ≤0.03 | 16.00~18.00 | 3.5~5.5 | – | – | 0.08 |
202 | ≤0.15 | ≤1.00 | 7.5~10.00 | ≤0.060 | ≤0.03 | 17.00~19.00 | 4.0~6.0 | – | ≤0.25 | |
301 | ≤0.15 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 16.00~18.00 | 6.00~8.00 | – | ||
302 | ≤0.15 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.03 | 17.00~19.00 | 8.00~10.00 | – | ||
304 | ≤0.07 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 18.00~20.00 | 8.00~10.50 | – | ||
304L | ≤0.030 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 18.00~20.00 | 9.00~13.00 | – | ||
310S | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 24.00~26.00 | 19.00~22.00 | – | ||
316 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 16.00~18.00 | 10.00~14.00 | 2.00~3.00 | ||
316L | ≤0.03 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 16.00~18.00 | 12.00~15.00 | 2.00~3.00 | ||
321 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 17.00~19.00 | 9.00~13.00 | – | ||
430 | ≤0.12 | ≤0.75 | ≤1.00 | ≤0.040 | ≤0.03 | 16.00~18.00 | – | |||
2205 | ≤0.03 | ≤1.00 | ≤2.00 | ≤0.030 | ≤0.015 | 22.00~23.00 | 4.5~6.5 | 2.5~3.5 | ||
2507 | ≤0.03 | ≤0.08 | ≤1.20 | ≤0.035 | ≤0.015 | 24.00~26.00 | 6.00~8.00 | 3.0~5.0 | ||
904L | ≤0.02 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.035 | 19.00~23.00 | 23.00~28.00 | 4.0~5.0 | 1.0~2.0 | |
INCONEL028 | ≤0.03 | ≤1.00 | ≤2.50 | ≤0.030 | ≤0.030 | ≤28.0 | ≤34.0 | ≤4.0 | ≤1.4 | |
MONEL400 | ≤0.30 | ≤0.5 | ≤2.00 | – | ≤0.024 | – | ≥63.0 | – | ≤34.0 | |
INCONEL800 | ≤0.10 | ≤1.00 | ≤1.50 | – | ≤0.015 | ≤23.0 | ≤35 | 4.0~5.0 | – | ≤0.75 |