Corrosion resistance
Titanium alloy design (0Cr18Ni10Ti) improves intergranular corrosion resistance and high temperature strength by adding titanium elements, and is suitable for chemical, petroleum and other industrial environments with high requirements for intergranular corrosion resistance.
High temperature strength
It can maintain stable performance in high temperature environments of 427-816°C, with a tensile strength of 515MPa and a yield strength of 205MPa, suitable for high temperature and high pressure scenes such as boiler pipes and heat exchangers.
Oxidation resistance
The addition of titanium enhances the antioxidant ability, especially suitable for industrial parts such as chemical pressure vessels and petroleum refining equipment that need to resist strong corrosive media such as nitric acid and sulfuric acid.
Organization stability
It can still maintain good organizational stability in high temperature environments, avoid performance degradation caused by grain boundary oxidation or phase change, and extend service life
Nombre del producto | Bobina/tira de acero inoxidable |
Estándar | ASTM,JIS,DIN,GB,AISI,DIN,EN |
Material | 201, 202, 301, 301L, 304, 304L, 316, 316L, 321, 310S, 904L, 410, 420J2, 430, 2205, 2507, 321H, 347, 347H, 403, 405, 409, 420, 430, 631, 904L, 305, 301L, 317, 317L, 309, 309S 310 |
Técnica | Estirado en frío, Laminado en caliente, Laminado en frío y Otros. |
Anchura | 6-12 mm o personalizable |
Espesor | 1-12 mm o personalizable |
Longitud | 1000 - 6000 mm o personalizable |
Tratamiento de superficies | BA/2B/NO.1/NO.3/NO.4/8K/HL/2D/1D |
Origen | China |
Código SA | 7219131200 |
Plazo de entrega | {Tiempo de entrega} |
Servicio posventa | 24 horas en línea |
Capacidad de producción | {Capacidad de producción} |
Condiciones de precio | EXW, FOB, CIF, CRF, CNF u otros. |
Puerto de carga | {Puerto} |
Plazo de pago | TT, LC,Efectivo, Paypal, DP, DA,Western Union u Otros. |
Aplicación | 1. Vajilla, armarios, tuberías interiores, calentadores de agua, calderas, bañeras |
2. Piezas de automóvil | |
3. Equipamiento médico, materiales de construcción, productos químicos, industria alimentaria, agricultura, componentes navales, etc. | |
Embalaje | Paquete, bolsa de PVC, cinturón de nylon, atadura de cables, paquete marítimo de exportación estándar o como petición. |
Servicio de tramitación | Doblado, soldadura, desbobinado, punzonado, corte y otros. |
Tolerancia | ±1% |
MOQ | {MOQ} |
Composición del acero inoxidable
El acero es una aleación de hierro y carbono. Los aceros inoxidables son aceros que contienen al menos 10,5% de cromo, menos de 1,2% de carbono y otros elementos de aleación. La resistencia a la corrosión del acero inoxidable y
Las propiedades mecánicas pueden mejorarse aún más añadiendo otros elementos, como níquel, molibdeno, titanio, niobio, manganeso, etc.
Grado | C | Si | Mn | P | S | Cr | Ni | Mo | N | Cu |
201 | ≤0.15 | ≤0.75 | 5.5~7.5 | ≤0.060 | ≤0.03 | 16.00~18.00 | 3.5~5.5 | – | – | 0.08 |
202 | ≤0.15 | ≤1.00 | 7.5~10.00 | ≤0.060 | ≤0.03 | 17.00~19.00 | 4.0~6.0 | – | ≤0.25 | |
301 | ≤0.15 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 16.00~18.00 | 6.00~8.00 | – | ||
302 | ≤0.15 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.03 | 17.00~19.00 | 8.00~10.00 | – | ||
304 | ≤0.07 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 18.00~20.00 | 8.00~10.50 | – | ||
304L | ≤0.030 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 18.00~20.00 | 9.00~13.00 | – | ||
310S | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 24.00~26.00 | 19.00~22.00 | – | ||
316 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 16.00~18.00 | 10.00~14.00 | 2.00~3.00 | ||
316L | ≤0.03 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 16.00~18.00 | 12.00~15.00 | 2.00~3.00 | ||
321 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 17.00~19.00 | 9.00~13.00 | – | ||
430 | ≤0.12 | ≤0.75 | ≤1.00 | ≤0.040 | ≤0.03 | 16.00~18.00 | – | |||
2205 | ≤0.03 | ≤1.00 | ≤2.00 | ≤0.030 | ≤0.015 | 22.00~23.00 | 4.5~6.5 | 2.5~3.5 | ||
2507 | ≤0.03 | ≤0.08 | ≤1.20 | ≤0.035 | ≤0.015 | 24.00~26.00 | 6.00~8.00 | 3.0~5.0 | ||
904L | ≤0.02 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.035 | 19.00~23.00 | 23.00~28.00 | 4.0~5.0 | 1.0~2.0 | |
INCONEL028 | ≤0.03 | ≤1.00 | ≤2.50 | ≤0.030 | ≤0.030 | ≤28.0 | ≤34.0 | ≤4.0 | ≤1.4 | |
MONEL400 | ≤0.30 | ≤0.5 | ≤2.00 | – | ≤0.024 | – | ≥63.0 | – | ≤34.0 | |
INCONEL800 | ≤0.10 | ≤1.00 | ≤1.50 | – | ≤0.015 | ≤23.0 | ≤35 | 4.0~5.0 | – | ≤0.75 |
Selección de superficies