Corrosion resistance
It performs well in oxidizing media (such as dilute nitric acid and dilute sulfuric acid), and also has good corrosion resistance to seawater and chloride solutions, but has poor corrosion resistance in alkaline media.
High temperature resistance
It can maintain stable performance at 427-816°C (800-1500°F), and the addition of titanium improves the resistance to intergranular corrosion at high temperatures.
Creep resistance
Ordinary 321 stainless steel may creep under long-term use at high temperatures, while high-carbon versions (such as 321H) show stronger creep resistance and are suitable for high-temperature environments.
Mechanical properties
Hardness: Brinell hardness about 201-217 HB, Rockwell hardness 85-92 HRB
Density: about 7.9 g/cm³
Melting point: 1375-1400°C
Application scenarios
Mainly used in industrial fields such as corrosion-resistant pipes, containers, and heat exchangers. Ordinary 321 stainless steel is suitable for medium and low temperature environments, while 321H is used in higher temperature scenarios (such as boilers and steam pipes)
Nombre del producto | Bobina/tira de acero inoxidable |
Estándar | ASTM,JIS,DIN,GB,AISI,DIN,EN |
Material | 201, 202, 301, 301L, 304, 304L, 316, 316L, 321, 310S, 904L, 410, 420J2, 430, 2205, 2507, 321H, 347, 347H, 403, 405, 409, 420, 430, 631, 904L, 305, 301L, 317, 317L, 309, 309S 310 |
Técnica | Estirado en frío, Laminado en caliente, Laminado en frío y Otros. |
Anchura | 6-12 mm o personalizable |
Espesor | 1-12 mm o personalizable |
Longitud | 1000 - 6000 mm o personalizable |
Tratamiento de superficies | BA/2B/NO.1/NO.3/NO.4/8K/HL/2D/1D |
Origen | China |
Código SA | 7219131200 |
Plazo de entrega | {Tiempo de entrega} |
Servicio posventa | 24 horas en línea |
Capacidad de producción | {Capacidad de producción} |
Condiciones de precio | EXW, FOB, CIF, CRF, CNF u otros. |
Puerto de carga | {Puerto} |
Plazo de pago | TT, LC,Efectivo, Paypal, DP, DA,Western Union u Otros. |
Aplicación | 1. Vajilla, armarios, tuberías interiores, calentadores de agua, calderas, bañeras |
2. Piezas de automóvil | |
3. Equipamiento médico, materiales de construcción, productos químicos, industria alimentaria, agricultura, componentes navales, etc. | |
Embalaje | Paquete, bolsa de PVC, cinturón de nylon, atadura de cables, paquete marítimo de exportación estándar o como petición. |
Servicio de tramitación | Doblado, soldadura, desbobinado, punzonado, corte y otros. |
Tolerancia | ±1% |
MOQ | {MOQ} |
Composición del acero inoxidable
El acero es una aleación de hierro y carbono. Los aceros inoxidables son aceros que contienen al menos 10,5% de cromo, menos de 1,2% de carbono y otros elementos de aleación. La resistencia a la corrosión del acero inoxidable y
Las propiedades mecánicas pueden mejorarse aún más añadiendo otros elementos, como níquel, molibdeno, titanio, niobio, manganeso, etc.
Grado | C | Si | Mn | P | S | Cr | Ni | Mo | N | Cu |
201 | ≤0.15 | ≤0.75 | 5.5~7.5 | ≤0.060 | ≤0.03 | 16.00~18.00 | 3.5~5.5 | – | – | 0.08 |
202 | ≤0.15 | ≤1.00 | 7.5~10.00 | ≤0.060 | ≤0.03 | 17.00~19.00 | 4.0~6.0 | – | ≤0.25 | |
301 | ≤0.15 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 16.00~18.00 | 6.00~8.00 | – | ||
302 | ≤0.15 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.03 | 17.00~19.00 | 8.00~10.00 | – | ||
304 | ≤0.07 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 18.00~20.00 | 8.00~10.50 | – | ||
304L | ≤0.030 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 18.00~20.00 | 9.00~13.00 | – | ||
310S | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 24.00~26.00 | 19.00~22.00 | – | ||
316 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 16.00~18.00 | 10.00~14.00 | 2.00~3.00 | ||
316L | ≤0.03 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 16.00~18.00 | 12.00~15.00 | 2.00~3.00 | ||
321 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 17.00~19.00 | 9.00~13.00 | – | ||
430 | ≤0.12 | ≤0.75 | ≤1.00 | ≤0.040 | ≤0.03 | 16.00~18.00 | – | |||
2205 | ≤0.03 | ≤1.00 | ≤2.00 | ≤0.030 | ≤0.015 | 22.00~23.00 | 4.5~6.5 | 2.5~3.5 | ||
2507 | ≤0.03 | ≤0.08 | ≤1.20 | ≤0.035 | ≤0.015 | 24.00~26.00 | 6.00~8.00 | 3.0~5.0 | ||
904L | ≤0.02 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.035 | 19.00~23.00 | 23.00~28.00 | 4.0~5.0 | 1.0~2.0 | |
INCONEL028 | ≤0.03 | ≤1.00 | ≤2.50 | ≤0.030 | ≤0.030 | ≤28.0 | ≤34.0 | ≤4.0 | ≤1.4 | |
MONEL400 | ≤0.30 | ≤0.5 | ≤2.00 | – | ≤0.024 | – | ≥63.0 | – | ≤34.0 | |
INCONEL800 | ≤0.10 | ≤1.00 | ≤1.50 | – | ≤0.015 | ≤23.0 | ≤35 | 4.0~5.0 | – | ≤0.75 |
Selección de superficies